AKJ150
Standard:
Size: 10-60
Description: ——
Application: ——
Typical Chemical Composition(%):
SiO₂+TiO₂: 14.0-23.0 CaO+MgO:24.0-36.0 S:0.035 P:0.04 CaF₂: 15.0-25.0 Al₂O₃+MnO:20.0-30.0
Notes on Usages:
1. The flux must be baked at 300°C~350°C for 2 hours before use.
2. Before welding, rust, oil, water and other impurities on the weldment should be removed.